Microstructural evaluation of Hastelloy-X transient liquid phase bonded joints: Effects of filler metal thickness and holding time
A. Malekan1, S. E. Mirsalehi2, M. Farvizi1, N. Saito3, K. Nakashima3

1. Ceramic Division, Materials and Energy Research Center, P.O. Box 14155-4777, Tehran, Iran;
2. Department of Materials and Metallurgical Engineering, Amirkabir University of Technology (Tehran Polytechnic), Tehran 15875-4413, Iran;
3. Department of Materials Science and Engineering, Kyushu University, 744, Motooka, Nishi-ku, Fukuoka 819-0395, Japan

Abstract:Transient liquid phase (TLP) bonding was investigated in Hastelloy-X samples with different filler metal thicknesses (20, 35, 50, 65, and 100 μm) and holding time (5, 20, 80, 320, and 640 min) to obtain optimum bonding parameters. Microstructural evaluations using electron probe microanalysis (EPMA) and electron backscattered diffraction (EBSD) show that the central eutectic phases present in the athermally solidified zone (ASZ) are Ni3B, Ni2Si, and CrB, and the precipitates formed in the diffusion-affected zone (DAZ) are MoB, CrB2, and Mo2B5. According to the results, decreasing the filler thickness as well as increasing the holding time helps realize the completion of isothermal solidification and reduction in the density of precipitates in the DAZ, leading to a joint with more uniform properties. Diffusion of boron and silicon to longer distances with increasing holding time causes the removal of Cr-rich borides in the DAZ and the formation of Mo-rich silicide at the joint interface. Decrease in hardness of ASZ and DAZ due to the elimination of brittle phases in these zones during long holding time causes more uniform hardness distribution in the joint area. The best results are obtained for the sample joined with the 35 μm-thick filler metal for 640 min holding time.

 

Key words: Hastelloy-X; transient liquid phase (TLP) bonding; microstructure; filler metal; electron probe microanalysis (EPMA); electron backscattered diffraction (EBSD)

ISSN 1004-0609
CN 43-1238/TG
CODEN: ZYJXFK

ISSN 1003-6326
CN 43-1239/TG
CODEN: TNMCEW

主管:中國科學(xué)技術(shù)協(xié)會 主辦:中國有色金屬學(xué)會 承辦:中南大學(xué)
湘ICP備09001153號 版權(quán)所有:《中國有色金屬學(xué)報》編輯部
------------------------------------------------------------------------------------------
地 址:湖南省長沙市岳麓山中南大學(xué)內(nèi) 郵編:410083
電 話:0731-88876765,88877197,88830410   傳真:0731-88877197   電子郵箱:f_ysxb@163.com  
延长县| 游戏| 米泉市| 调兵山市| 山东省| 修文县| 德江县| 昌吉市| 三穗县| 湘西| 鹤山市| 甘洛县| 庐江县| 宁城县| 宜昌市| 隆安县| 太仆寺旗| 南川市| 汝城县| 米林县| 宁陕县| 堆龙德庆县| 普兰县| 称多县| 城市| 乌鲁木齐市| 洛阳市| 东至县| 龙岩市| 西丰县| 万全县| 文安县| 政和县| 赤峰市| 靖安县| 长武县| 龙南县| 布尔津县| 天门市| 渑池县| 郯城县|